Schierle Siyaya
Ferritic heat-resistant

1.4742

TP 430

X10CrAlSi18

Aluminium-silicon ferritic heat-resistant steel with good resistance to sulphur-bearing gases to about 1000 °C.

Chemical composition

mass %
ElementContent
CCarbon≤0.12
SiSilicon0.7–1.4
MnManganese≤1
PPhosphorus≤0.04
SSulphur≤0.03
AlAluminium0.7–1.2
CrChromium17–19

Mechanical properties

room temperature
Scaling temperature (°C)
1000

Standard equivalences

DIN/EN
X10CrAlSi18
AISI
430 (heat-resistant)
AFNOR
Z10 CAS 18
PN
H18JS

Typical applications

  • Furnaces and gas turbines
  • Exhaust valves and thermowell tubes
  • Power-plant and reactor construction
  • Heat exchangers, muffle tubes, recuperators

Frequently asked questions

What is 1.4742 (TP 430)?

1.4742 (X10CrAlSi18) — Ferritic heat-resistant. Aluminium-silicon ferritic heat-resistant steel with good resistance to sulphur-bearing gases to about 1000 °C.

Which grades are equivalent to 1.4742?

1.4742 corresponds to EN X10CrAlSi18; equivalent designations: AISI 430 (heat-resistant), AFNOR Z10 CAS 18, PN H18JS.

Related grades

Indicative values — verify against the applicable standard before specifying.

Request this grade