Schierle Siyaya
Austenitic heat-resistant

1.4835

253 MA

X9CrNiSiNCe21-11-2

High-temperature austenitic with nitrogen and rare-earth additions for raised strength, oxidation and corrosion resistance at 850–1100 °C.

Chemical composition

mass %
ElementContent
CCarbon0.05–0.12
SiSilicon1.4–2.5
MnManganese≤1
CrChromium20–22
NiNickel10–12
NNitrogen0.12–0.2
CeCerium0.03–0.08

Mechanical properties

room temperature
Scaling temperature (°C)
1100

Standard equivalences

DIN/EN
X9CrNiSiNCe21-11-2
AISI
253 MA
UNS
S30815

Typical applications

  • Power-plant construction
  • Oil and petrochemical service
  • Furnace construction: heat exchangers, air preheaters, recuperators
  • Furnace and cracker tubes, thermowell tubes

Frequently asked questions

What is 1.4835 (253 MA)?

1.4835 (X9CrNiSiNCe21-11-2) — Austenitic heat-resistant. High-temperature austenitic with nitrogen and rare-earth additions for raised strength, oxidation and corrosion resistance at 850–1100 °C.

Which grades are equivalent to 1.4835?

1.4835 corresponds to EN X9CrNiSiNCe21-11-2; equivalent designations: AISI 253 MA, UNS S30815.