Schierle Siyaya
Austenitic heat-resistant

1.4919

TP 316H

X6CrNiMo17-13

Controlled-carbon 316 for elevated-temperature service (316H) with improved creep strength for pressure parts.

Chemical composition

mass %
ElementContent
CCarbon0.04–0.08
SiSilicon≤0.75
MnManganese≤2
CrChromium16–18
MoMolybdenum2–2.5
NiNickel12–14
PPhosphorus≤0.035
SSulphur≤0.015

Mechanical properties

room temperature
Rp0.2 min (N/mm²)
205
Rm (N/mm²)
490–690
Elongation A% (longitudinal)
35

A measured at L0 = 5 d0.

Standard equivalences

DIN/EN
X6CrNiMo17-13
AISI
316H
UNS
S31609
AFNOR
X6CrNiMoB17-12-2
BS
316 S50

Typical applications

  • Power-plant and reactor construction
  • Components for thermal power plant
  • Valves, discs, housings
  • Superheater, heat-exchanger and steam-line tubes

Frequently asked questions

What is 1.4919 (TP 316H)?

1.4919 (X6CrNiMo17-13) — Austenitic heat-resistant. Controlled-carbon 316 for elevated-temperature service (316H) with improved creep strength for pressure parts.

Which grades are equivalent to 1.4919?

1.4919 corresponds to EN X6CrNiMo17-13; equivalent designations: AISI 316H, UNS S31609, AFNOR X6CrNiMoB17-12-2, BS 316 S50.

Related grades

Indicative values — verify against the applicable standard before specifying.

Request this grade